Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Rear Barrel Temperature | 177 - 191 °C | 351 - 376 °F | |
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |