Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 165 - 180 °C | 329 - 356 °F | |
KEP Kepital® F20 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 165 - 180 °C | 329 - 356 °F | |
KEP Kepital® F20-52 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 165 - 180 °C | 329 - 356 °F | |
KEP Kepital® F30 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 165 - 180 °C | 329 - 356 °F | |
KEP Kepital® FG2025 25% Glass Fiber Reinforced Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 165 - 185 °C | 329 - 365 °F | |
Huntsman AVALON® 65 AC Thermoplastic Polyurethane Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia.. |
|||
Rear Barrel Temperature | 165 °C | 329 °F | Injection |
Alliance Polymers Zythane™ 4060A Thermoplastic Polyurethane Elastomer Zythane™ 4060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Rear Barrel Temperature | 165 °C | 329 °F | Injection |
Alliance Polymers Zythane™ 5060A Thermoplastic Polyurethane Elastomer Zythane™ 5060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Rear Barrel Temperature | 165 °C | 329 °F | Injection |
Alliance Polymers Zythane™ 6070A Thermoplastic Polyurethane Elastomer Zythane™ 6070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Rear Barrel Temperature | 165 °C | 329 °F | Injection |
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |