Processing Properties Metric English Comments
Rear Barrel Temperature 138 - 154 °C
280 - 310 °F
RheTech Products E206-01 Linear Low Density Polyethylene, Black
Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 138 °C
280 °F
Advanced Elastomer Systems VistaFlex® 641N Thermoplastic Rubber  (discontinued **)
A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vica..
Rear Barrel Temperature 138 °C
280 °F
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber  (discontinued **)
A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 9.0 MPa (1300 psi); Vica..
Rear Barrel Temperature 138 - 216 °C
280 - 420 °F
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 138 - 160 °C
280 - 320 °F
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer
Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit..
Rear Barrel Temperature 138 - 160 °C
280 - 320 °F
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer
Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and ..