Processing Properties Metric English Comments
Rear Barrel Temperature 192 - 215 °C
378 - 419 °F
Start Point: 200°C
Kingfa FRHIPS-702 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing..
Rear Barrel Temperature 175 - 215 °C
347 - 419 °F
Blow Molding
LG Chemical HYPERIER IP1306B PA-HDPE Nanoclay Compound
HYPERIER is a nano compound made from nano-sized inorganic plate clay. Blow Molding, Barrier thermoplastic, Nylon blend with HDPEApplication: Agrochemical Container, SORE* Fuel Tank, PFCCAS No. 900..
Rear Barrel Temperature 192 - 215 °C
378 - 419 °F
Start Point: 200°C
Kingfa FRHIPS-722 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing..