Processing Properties Metric English Comments
Rear Barrel Temperature 192 - 215 °C
378 - 419 °F
Start Point: 200°C
Kingfa FRHIPS-702 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing..
Rear Barrel Temperature 192 - 215 °C
378 - 419 °F
Start Point: 200°C
Kingfa FRHIPS-722 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing..