Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 163 - 168 °C | 325 - 335 °F | |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most .. |