Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Trilliant™ HC X HC5200-0028 XR Gray Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7930-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7690-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7930-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7960-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar MN200 Copolyester Eastar Copolyester MN200 is an amorphous copolyester with excellent flow characteristics as well as radiation resistance and chemical resistance.Applications/UsesMedical |
|||
Mold Temperature | 10.0 - 38.0 °C | 50.0 - 100 °F | |
Ecomass® 4450CI86 Carbonyl Iron Filled Polypropylene Nontoxic alternative to Lead (Pb), for shielding applicationsHigh Specific GravityCarbonyl Iron Filled Polypropylene Random Co-PolymerInformation provided by Technical Polymers |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Clariant Renol PPSP0017 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® 8088N Thermoplastic Elastomer Elastocon® 8088N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8088N is FDA compliant and well suited.. |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer Elastocon® 8138B is a black thermoplastic elastomer compound formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8138B is well suited for consumer.. |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® CLR75 Thermoplastic Elastomer Elastocon® CLR75 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a tactile surface fin.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.0 - 100 °F | |
PolyOne Edgetek® UR-30GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |