Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Injection Molding |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® OBC 4530A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1025-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1154A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1155B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1183A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1431F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1522A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1654D Thermoplastic Elastomer Notes: Non-halogenated; RoHS Compliant; MBDC: Green Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General .. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1654G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-2565A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-2575F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-2069B Thermoplastic Elastomer Uses: Caps; Food Packaging; Liners Pellets Processing Method: Extrusion; Injection Molding; Press Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmIn.. |
|||
Mold Temperature | 25.0 - 60.0 °C | 77.0 - 140 °F | |
Arkema Group Rilsan® PA 11 G BMNO MED Nylon 11 Rilsan® PA 11 G BMNO MED is a polyamide produced from a renewable source. This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applic.. |