Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 54.4 - 71.1 °C | 130 - 160 °F | Cavity mold surface temperature at equilibrium conditions |
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin Features: Ultra high modulus, High heat resistance, excellent adhesion to urethaneApplications: Instrument panel substrates, Brackets, Structural components |
|||
Mold Temperature | 54.4 - 65.6 °C | 130 - 150 °F | |
PolyOne Edgetek® AS-20GF-05GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |