Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 161J-1 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 161J1-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 202 - 213 °C | 396 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 161J-1-3V/2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 161J-4-DD Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 161JA White Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 2121 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 202 - 213 °C | 396 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 2160 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 202 - 213 °C | 396 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 2188GC Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 202 - 213 °C | 396 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 2188GC-1V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 202 - 213 °C | 396 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 202 - 213 °C | 396 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 2188NT Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent natural PVC bottle compound for blow molding applications.Information provided by PolyOne |
|||
Mold Temperature | 202 - 213 °C | 396 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 2320 LCW Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 4195 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 01FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 13FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging PK8-1080 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging PK9 WHITE 1082 Polyvinyl Chloride, Rigid (PVC, Rigid) The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne |
|||
Mold Temperature | 202 - 213 °C | 396 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging UV-SORB-1 Polyvinyl Chloride, Rigid (PVC, Rigid) Caution: To be used as an additive only.Bottles produced from blends of OxyClear UV-SORB-1 are specifically designed for use where UV sensitive products are being packaged. Dependent on the base Oxy.. |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging VB9-51 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |