Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 163 - 218 °C | 325 - 425 °F | Average value: 190 °C Grade Count:13 |
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and .. |
|||
Mold Temperature | 163 - 168 °C | 325 - 335 °F | |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most .. |