Processing Properties Metric English Comments
Nozzle Temperature 357 - 382 °C
675 - 720 °F
Oxford Polymers PEEK-20CF-Black PEEK, 20% Carbon Fiber Reinforced
Product Description: Carbon Fiber (20% Reinforced), PEEK, Polyetheretherketone, injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon fiber Special Ch..
Nozzle Temperature 360 - 382 °C
680 - 720 °F
Oxford Polymers PEI 1000 PEI
Product Description: (Unreinforced), Polyetherimide injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Colors AvailableInformation provided..
Nozzle Temperature 360 - 382 °C
680 - 720 °F
Oxford Polymers PEI 1010 PEI
Product Description: (Unreinforced), Polyetherimide injection molding grade, high flow Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: ..