Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 188 - 207 °C | 370 - 405 °F | |
PolyOne Dynaflex™ G2780-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G2780-0001 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmo.. |
|||
Nozzle Temperature | 188 - 227 °C | 370 - 441 °F | |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Nozzle Temperature | 188 - 221 °C | 370 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Nozzle Temperature | 188 - 221 °C | 370 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 4445 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4445 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® OBC 4470A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® OBC 4545A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® OBC 4565A Thermoplastic Elastomer Uses: Flexible Grips; Overmolding Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion; Extrusion; Injection Molding Injection .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1025-85 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1035-70UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1269A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1336 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1336A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1420C Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Injecti.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1522E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1642E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1654B Thermoplastic Elastomer Notes: Non-halogenated Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstr.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-2433A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-2535F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-6055 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-81-D965-P Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-87-L832A Thermoplastic Elastomer Notes: UV Stabilized Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstrip.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-88-N873K BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-89-P808A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-91-T3056S-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-2468A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-2580A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer Elastocon® 8138B is a black thermoplastic elastomer compound formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8138B is well suited for consumer.. |
|||
Nozzle Temperature | 188 - 221 °C | 370 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Nozzle Temperature | 188 - 221 °C | 370 - 430 °F | |
ExxonMobil Santoprene® 171-55 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Nozzle Temperature | 188 - 221 °C | 370 - 430 °F | |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |