Processing Properties | Metric | English | Comments |
---|---|---|---|
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-1586UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-1698 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-2123 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-2207B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-2315 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP 1056 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-1358D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-1393A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-2359A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-2820M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-3017 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-3955B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® OBC 2318D Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® OBC 4873A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-1025-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-1269B Thermoplastic Elastomer Uses: Consumer Applications; Handles; Packaging; General Purpose; Kitchenware; Toothbrush Handles Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Mode.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-1420A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-1642E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-2530F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-2545A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-6055 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-6800-73 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-83-F912-E-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-89-P808A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Uniprene® UN-1373G Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-1934F Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Connectors; Wire Jacketing Agency Ratings: UL 1581Forms: Pellets Processing Method: Extrusion; Injec.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Telcar® TL-2468A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-2750 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
Teknor Apex Monprene® MP-2830M UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |