Polymer Property : Injection Velocity = 1.97 in/sec Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Velocity 50.0 - 150 mm/sec
1.97 - 5.91 in/sec
Average value: 100 mm/sec Grade Count:7
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Injection Velocity 50.0 mm/sec
1.97 in/sec
Injection molding
Styrolution Styrolux 3G55 SBC
Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex..
Injection Velocity 50.0 mm/sec
1.97 in/sec
Injection molding
Styrolution Styrolux 684D SBC
Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and..
Injection Velocity 50.0 - 150 mm/sec
1.97 - 5.91 in/sec
Moderate to Fast
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che..
Injection Velocity 50.0 - 150 mm/sec
1.97 - 5.91 in/sec
Moderate to Fast
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high ..
Injection Velocity 50.0 - 150 mm/sec
1.97 - 5.91 in/sec
Moderate to Fast
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,..
Injection Velocity 50.0 - 150 mm/sec
1.97 - 5.91 in/sec
Moderate to Fast
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture..
Injection Velocity 50.0 - 150 mm/sec
1.97 - 5.91 in/sec
Moderate to Fast
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
Injection Velocity 50.0 - 150 mm/sec
1.97 - 5.91 in/sec
Moderate to Fast
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC)
TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist..
Injection Velocity 50.0 mm/sec
1.97 in/sec
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF
A chemically coupled 40% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ G90A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G90A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ P75A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P75A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ P80A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ P90A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P90A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity >= 50.0 mm/sec
>= 1.97 in/sec
Injection
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Injection Velocity 50.0 mm/sec
1.97 in/sec
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF
A chemically coupled 30% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Injection Velocity 50.0 mm/sec
1.97 in/sec
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF
A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.