Processing Properties Metric English Comments
Front Barrel Temperature 171 - 182 °C
340 - 360 °F
Green Dot Terratek® BD 4015 Biodegradable Polymer
Terratek BD biodegradable composites are created from a proprietary blend of starch-based ingredients and other materials, the natural components derived from renewable grain sources account for the..
Front Barrel Temperature 166 - 182 °C
330 - 360 °F
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer
Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit..
Front Barrel Temperature 166 - 182 °C
330 - 360 °F
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer
Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and ..
Front Barrel Temperature 166 - 182 °C
330 - 360 °F
Elastocon TPE Technologies Elastocon® 2855 Thermoplastic Elastomer
Elastocon® 2855 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2855 is FDA compliant and well suited for cons..
Front Barrel Temperature 160 - 182 °C
320 - 360 °F
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer
Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited..
Front Barrel Temperature 177 - 182 °C
350 - 360 °F
Elastocon TPE Technologies Elastocon® 8068B Thermoplastic Elastomer
Elastocon® 8068B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068B is well suited for consumer goods an..
Front Barrel Temperature 177 - 182 °C
350 - 360 °F
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer
Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well sui..
Front Barrel Temperature 177 - 182 °C
350 - 360 °F
Elastocon TPE Technologies Elastocon® 8068L Thermoplastic Elastomer
Elastocon® 8068L is a colorable lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068L is well ..
Front Barrel Temperature 177 - 182 °C
350 - 360 °F
Elastocon TPE Technologies Elastocon® 8068N Thermoplastic Elastomer
Elastocon® 8068N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068N is FDA compliant and well suited..
Front Barrel Temperature 160 - 182 °C
320 - 360 °F
Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer
Elastocon® 8138B is a black thermoplastic elastomer compound formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8138B is well suited for consumer..