Processing Properties Metric English Comments
Front Barrel Temperature 326 - 339 °C
619 - 642 °F
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA), 33% Glass Fiber
Amodel® A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment...
Front Barrel Temperature 326 - 339 °C
619 - 642 °F
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber
Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e..
Front Barrel Temperature 326 - 339 °C
619 - 642 °F
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi..