Polymer Property : Front Barrel Temperature = 241 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 229 - 241 °C
445 - 465 °F
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 229 - 241 °C
445 - 465 °F
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 229 - 241 °C
445 - 465 °F
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).