Processing Properties Metric English Comments
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Ecobarrier™ 0414 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Ecobarrier™ 0512 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Ecobarrier™ 0712 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Ecobarrier™ 0914 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Ecobarrier™ 0916 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Forte™ 35CP091 Nanocomposite
Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Forte™ 4CPP093 Nanocomposite
Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Regis™ 125098 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Regis™ 230106 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Regis™ 235107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Regis™ 285107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Regis™ 315107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Regis™ 190108 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Noble Polymers Regis™ 225104 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-003 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-005 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-026 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-028 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-046 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-050 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-051 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-072 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-081 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-082 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-085 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-089 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-091 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-116 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-214 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
CPT C-Flex® R70-190 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..