Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 154 - 171 °C | 310 - 340 °F | |
RheTech Products E204-01 High Density Polyethylene, Black Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 154 - 171 °C | 310 - 340 °F | |
RheTech Products E204-00 High Density Polyethylene, Natural Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |