Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 351 - 390 °F | |
PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE) Versaflex™ OM 2262 is a performance overmolding grade with general FDA compliance. This product is designed for both insert and two-shot molding onto Eastman Tritan™ copolyester as well as ABS, PC.. |
|||
Middle Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® CR-92-E2555A-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® OBC 4560A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® OBC 4855A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® OBC 4876N Thermoplastic Elastomer Uses: Flexible Grips; Overmolding; Soft Touch Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL 2530A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1025-65 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1025-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1035-70UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1155A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1221A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1336A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1402G Thermoplastic Elastomer Notes: Non-halogenated, Flame Retardant TPE; RoHS Compliant Uses: Connectors; Electrical/Electronic Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injec.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1420C Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Injecti.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1431A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1431F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1488G Thermoplastic Elastomer Uses: Flexible Grips; General Purpose; Handles; Household Goods; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1536D Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Household Goods; Food Containers; Handles; Lids Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2503S Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2507B Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2565F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2597 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2635C Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-340-S Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-90-T3030A-80 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1996E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-8732 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-91-T3056S-90 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |