Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 360 - 377 °C | 680 - 711 °F | |
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU) Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn.. |
|||
Middle Barrel Temperature | 360 - 377 °C | 680 - 711 °F | |
Solvay Specialty Polymers Radel® R-7400 Polyphenylsulfone (PPSU) Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame.. |
|||
Middle Barrel Temperature | 360 - 377 °C | 680 - 711 °F | |
Solvay Specialty Polymers Radel® R-7535 Polyphenylsulfone (PPSU) Radel® R-7535 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu.. |
|||
Middle Barrel Temperature | 360 - 377 °C | 680 - 711 °F | |
Solvay Specialty Polymers Radel® R-7558 Polyphenylsulfone (PPSU) Radel® R-7558 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu.. |
|||
Middle Barrel Temperature | 360 - 377 °C | 680 - 711 °F | |
Solvay Specialty Polymers Radel® R-7625 Polyphenylsulfone (PPSU) Radel® R-7625 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications that offers improved UV resistance versus Radel® R-7535 and Radel® R-7558. The product .. |
|||
Middle Barrel Temperature | 360 - 377 °C | 680 - 711 °F | |
Solvay Specialty Polymers Radel® R-7300 Polyphenylsulfone (PPSU) Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame r.. |