Polymer Property : Sintering Temperature = 3137 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Sintering Temperature 1725 °C
3137 °F
Nabaltec NABALOX® NO 615-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Sintering Temperature 1725 °C
3137 °F
Nabaltec NABALOX® NO 615-30 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Sintering Temperature 1725 °C
3137 °F
Nabaltec NABALOX® NO 625-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Sintering Temperature 1725 °C
3137 °F
Nabaltec NABALOX® NO 625-30 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Sintering Temperature 1725 °C
3137 °F
Nabaltec NABALOX® NO 625-31 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Sintering Temperature 1725 °C
3137 °F
Nabaltec NABALOX® NO 715-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Sintering Temperature 1725 °C
3137 °F
Nabaltec NABALOX® NO 725-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..