Processing Properties | Metric | English | Comments |
---|---|---|---|
Sintering Temperature | 550 - 750 °C | 1020 - 1380 °F | |
Gwent Electronic Materials C2030922D1 Silver Ink Silver Ink C2030922D1 is a grey ink with a pine smell at a ready to use viscosity suitable for firing on glass and ceramic to form conductive tracks. The ink should be gently stirred before use avo.. |
|||
Sintering Temperature | 550 - 625 °C | 1020 - 1160 °F | |