Polymer Property : Cure Time = 2.50 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 120 - 150 min

@Temperature 93.3 °C
2.00 - 2.50 hour

@Temperature 200 °F
Master Bond EP21AR Acid Resistant Two Component Epoxy
Master Bond EP21AR is a two component epoxy resin compound for durable, high performance, coating liner and adhesive/sealant with outstanding acid as well as excellent overall chemical resistance. E..
Cure Time 120 - 150 min

@Temperature 93.3 °C
2.00 - 2.50 hour

@Temperature 200 °F
Master Bond EP30D-7 Flexibilized, Abrasion Resistant Epoxy System
Master Bond Polymer System EP30D-7 is a versatile two component flexibilized, urethane-modified epoxy featuring superior strength, toughness and abrasion resistance for high performance bonding, sea..