Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 105 min @Temperature 100 °C |
1.75 hour @Temperature 212 °F |
|
Dow Corning 3-4154 DIELECTRIC GEL KIT Two-part, clear, RT or heat cure.Information provided by Dow Corning |
|||
Cure Time | 105 min @Temperature 24.0 °C |
1.75 hour @Temperature 75.2 °F |
Dry to Touch Time; ASTM D1640 clause 7.5.2 |
3M Scotchkote™ 323 Purple Patch Compound 3M Scotchkote 323 Purple Patch Compound is an ambient temperature cure, two-part system designed to protect metal, concrete and other surfaces from corrosion and deterioration. Scotchkote 323 Purple.. |
|||
Cure Time | 105 min @Temperature 24.0 °C |
1.75 hour @Temperature 75.2 °F |
ASTM D1640 |
3M Scotchkote™ 323R Liquid Epoxy Coating 3M Scotchkote Rebar Liquid Patch Compound 323R is a two-part, ambient temperature cure, 100% solids content, thermosetting, liquid epoxy coating. Intended Uses:As a patch materialAs a rebar shear en.. |