Polymer Property : Cure Time = 0.125 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 7.50 min

@Temperature 100 °C
0.125 hour

@Temperature 212 °F
Dow Corning 3-4130 DIELECTRIC GEL KIT
Two-part, clear, heat cure, low extractables.Information provided by Dow Corning
Cure Time 7.50 min

@Temperature 150 °C
0.125 hour

@Temperature 302 °F
Dow Corning 3-4237 DIELECTRIC FIRM GEL KIT
Two-part, translucent green, heat cure, firm, long working time, primerless chemical adhesion.Information provided by Dow Corning