Polymer Property : Cure Time = 0.0733 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 4.40 min

@Temperature 155 °C
0.0733 hour

@Temperature 311 °F
ts2
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 4.40 min

@Temperature 155 °C
0.0733 hour

@Temperature 311 °F
ts2
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 6.0 PHR MBTS
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 4.40 min

@Temperature 155 °C
0.0733 hour

@Temperature 311 °F
ts2
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 4.40 min

@Temperature 155 °C
0.0733 hour

@Temperature 311 °F
ts2
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 6.0 PHR MBTS
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..