Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 120 - 150 min @Temperature 93.3 °C |
2.00 - 2.50 hour @Temperature 200 °F |
|
Master Bond EP21AR Acid Resistant Two Component Epoxy Master Bond EP21AR is a two component epoxy resin compound for durable, high performance, coating liner and adhesive/sealant with outstanding acid as well as excellent overall chemical resistance. E.. |
|||
Cure Time | 120 - 150 min @Temperature 93.3 °C |
2.00 - 2.50 hour @Temperature 200 °F |
|
Master Bond EP30D-7 Flexibilized, Abrasion Resistant Epoxy System Master Bond Polymer System EP30D-7 is a versatile two component flexibilized, urethane-modified epoxy featuring superior strength, toughness and abrasion resistance for high performance bonding, sea.. |