Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 6.00 - 42.0 min @Temperature 25.0 °C |
0.100 - 0.700 hour @Temperature 77.0 °F |
De-mold Time |
Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for th.. |
|||
Cure Time | 6.00 min @Temperature 130 °C |
0.100 hour @Temperature 266 °F |
|
Resin Technology Group TIGA 905 One-Part Silver Conductive Epoxy System Cure 6 minutes at 130°C or 3 minutes at 150°C.TIGA 905 is a stress-absorbing and electrically conductive, silver-filled epoxy adhesive recommended for solder replacement in microelectronic interco.. |
|||
Cure Time | 6.00 min @Temperature 160 °C |
0.100 hour @Temperature 320 °F |
|
Trelleborg Emerson & Cuming Eccobond® D 275 One-Component Fast Cure Epoxy Adhesive Emerson & Cuming D 275 Eccobond® One-Component Fast Cure Epoxy AdhesiveSemi-rigid, high strength, fast curing, pourable, epoxy structural adhesive. Good peel strength (12 pli), Recommended for bond.. |
|||
Cure Time | 6.00 min @Temperature 204 °C |
0.100 hour @Temperature 399 °F |
|
3M Scotchcast™ 5230N Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 5230N is a widely used, general purpose epoxy powder resin. A one-part, blue pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moistu.. |
|||
Cure Time | 6.00 min @Temperature 204 °C |
0.100 hour @Temperature 399 °F |
|
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 5388 is a one-part, blue pigmented, rapid heat curing powder resin, designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a var.. |
|||
Cure Time | 6.00 min @Temperature 177 °C |
0.100 hour @Temperature 351 °F |
|
3M Scotchcast™ 5555 10G Electrical Insulating Epoxy Resin 3M Scotchcast Electrical Resin 5555 is a one-part, green pigmented, rapid heat curing powder coating. It is designed to provide a continuous, tough moisture and chemical resistant dielectric coating.. |
|||
Cure Time | 6.00 min @Temperature 218 °C |
0.100 hour @Temperature 424 °F |
|
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade) 3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheate.. |
|||
Cure Time | 6.00 min @Temperature 218 °C |
0.100 hour @Temperature 424 °F |
|
3M Scotchkote™ 412 Spray Grade Fusion Bonded Epoxy Coating 3M Scotchkote Spray Grade Fusion Bonded Epoxy Coating 413 is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of reinforcing steel. The epoxy is applied to pre.. |
|||
Cure Time | 6.00 min @Temperature 140 °C |
0.100 hour @Temperature 284 °F |
Dry to stack, at 50% humidity |
Blue River Coatings Wood Primer BLUE RIVER COATINGGS WOOD PRIMER is a high quality, single component primer, not requiring any catalyzing agent. WOOD PRIMER offers good coverage, excellent durability, and ease of application, as w.. |