Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 5.00 - 40.0 MPa @Time 10.0 - 30.0 sec |
725 - 5800 psi @Time 0.00278 - 0.00833 hour |
|
Gromax 1140LH TPE Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject.. |
|||
Hold Pressure | 5.00 - 40.0 MPa @Time 10.0 - 30.0 sec |
725 - 5800 psi @Time 0.00278 - 0.00833 hour |
|
Gromax 1155LL TPE 1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex.. |
|||
Hold Pressure | 5.00 - 40.0 MPa @Time 10.0 - 30.0 sec |
725 - 5800 psi @Time 0.00278 - 0.00833 hour |
|
Gromax 1163LL TPE 163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext.. |
|||
Hold Pressure | 5.00 - 40.0 MPa @Time 10.0 - 30.0 sec |
725 - 5800 psi @Time 0.00278 - 0.00833 hour |
|
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |