Polymer Property : Casting Temperature = 1810 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Casting Temperature 990 - 1090 °C
1810 - 1990 °F
Wieland 1114 Wilaform Gold
Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental
Casting Temperature 990 - 1190 °C
1810 - 2170 °F
Wieland 1604 Wilaform Gold
Rose gold for all kinds of decoration manufacturingApplications: casting, laminar decoration, pipes, tubingDental
Casting Temperature 990 - 1090 °C
1810 - 1990 °F
Wieland 1608 Wilaform Gold
Universally applicable yellow gold alloy.Applications: casting, chains, laminar decoration, pipes, tubingDental