Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 250 °C | 482 °F | Die |
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound PRE-ELEC® PP 1396 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Zone 4 | 250 - 285 °C | 482 - 545 °F | |
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6 Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo.. |
|||
Zone 4 | 250 °C | 482 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Zone 4 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 64C-R Nylon 66, DAM Vydyne® 64C-R is a medium-viscosity PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. Vydyne 64C-R resin offers high strength.. |
|||
Zone 4 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, DAM Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h.. |
|||
Zone 4 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, .. |
|||
Zone 4 | 250 °C | 482 °F | Nozzle |
BASF Ultradur® B 4406 PBT Description: Is a PBT, flame-retardant injection-molding grades, unreinforced for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting compo.. |
|||
Zone 4 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 66Z Nylon 66, DAM Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug.. |
|||
Zone 4 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, DAM Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and.. |
|||
Zone 4 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, DAM Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, .. |
|||
Zone 4 | 250 °C | 482 °F | Nozzle |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Zone 4 | 250 °C | 482 °F | Nozzle |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |