Polymer Property : Zone 4 = 401 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 205 °C
401 °F
SK Chemicals SKYTHANE® L194A Polycaprolactone Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Zone 4 205 °C
401 °F
SK Chemicals SKYTHANE® R155D Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Zone 4 205 °C
401 °F
SK Chemicals SKYTHANE® S155D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Zone 4 205 °C
401 °F
Borealis Borcell™ HE4873 High Density Polyethylene
Borcell™ HE4873 is a fully formulated compound for physical foamed data cable insulation. Borcell™ HE4873 is a high-density polyethylene compound containing blowing agent for the production of foa..
Zone 4 205 °C
401 °F
Extrusion
Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane
Features: High stiffness TPU alloyUses: Flat Die/Cast Sheet Extrusion, Profile Extrusion and Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided b..
Zone 4 205 - 215 °C
401 - 419 °F
Injection
Lubrizol Estane® GP 55 DB Thermoplastic Polyurethane
Type: Estane® GP 55DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding partsAvailable in EuropeInformation Provided by..
Zone 4 205 - 215 °C
401 - 419 °F
Injection
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane
Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 4 205 - 215 °C
401 - 419 °F
Injection
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
Zone 4 205 °C
401 °F
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin
EPDA-5040 is a high molecular weight high density polyethylene copolymer resin designed for non-pressure gravity pipe applications. It has a good balance of flexibility, ductility, stiffness and tou..
Zone 4 205 - 230 °C
401 - 446 °F
Arkema Group OREVAC® 18760 Grafted Maleic Anhydride Polypropylene
OREVAC 18760 is a maleic anhydride grafted polypropylene used in the manufacturing of three layer PP coating for steel pipeline. OREVAC 18760 is also used in multilayer EVOH – PP structures. OREVAC..
Zone 4 205 - 215 °C
401 - 419 °F
Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane  (discontinued **)
PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio..