Polymer Property : Zone 4 = 330 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 166 °C
330 °F
Axiall HHP-190 Rigid PVC, Extrusion
Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensi..
Zone 4 166 °C
330 °F
Axiall HHW-191 Rigid PVC, Extrusion
Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic..
Zone 4 166 °C
330 °F
Axiall Tuf-Stif 2802 Rigid PVC, Extrusion
Georgia Gulf Tuf-Stif 2802 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit..
Zone 4 166 °C
330 °F
Axiall Tuf-Stif 2804 Rigid PVC, Extrusion
Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit..