Polymer Property : Zone 4 = 320 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Polidan® EC/110 Polyethylene, Crosslinked (XLPE)
Polidan® XLPE-PEX -Cross-linkable Polyethylene. Low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be use..
Zone 4 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Polidan® EC/51 Polyethylene, Crosslinked (XLPE)
Flexible low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards com..