Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 160 - 180 °C | 320 - 356 °F | |
Solvay Specialty Polymers Polidan® EC/110 Polyethylene, Crosslinked (XLPE) Polidan® XLPE-PEX -Cross-linkable Polyethylene. Low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be use.. |
|||
Zone 4 | 160 - 180 °C | 320 - 356 °F | |
Solvay Specialty Polymers Polidan® EC/51 Polyethylene, Crosslinked (XLPE) Flexible low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards com.. |