Processing Properties Metric English Comments
Zone 3 165 - 175 °C
329 - 347 °F
Extrusion Molding
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane
ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon.
Zone 3 165 - 170 °C
329 - 338 °F
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane
Pearlbondâ„¢ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus..
Zone 3 165 - 175 °C
329 - 347 °F
Lubrizol Advanced Materials PEARLTHANE® 12F75UV Thermoplastic Polyurethane Elastomer
PEARLTHANE® D12F75UV is a UV resistant standard polyester based TPU supplied in form of translucent, colorless or slightly yellowish pellets, featuring a low melting point and very low gel conten..
Zone 3 165 °C
329 °F
Lubrizol Estane® ALR G500 Water Absorbent Thermoplastic Polyurethane
Type: Estane® ALR G500 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provide..