Processing Properties Metric English Comments
Zone 3 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 3 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 3 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 3 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 3 170 - 180 °C
338 - 356 °F
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1..
Zone 3 170 - 180 °C
338 - 356 °F
Injection Molding
Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionHighly Pressurized Hose Information provided by API-Kolon.
Zone 3 170 - 180 °C
338 - 356 °F
Injection Molding
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane
ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon.
Zone 3 170 - 180 °C
338 - 356 °F
Lubrizol Advanced Materials PEARLCOAT® 127K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 127K is a polyester based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and medium softening point. PEARLCOATÂ..
Zone 3 170 - 180 °C
338 - 356 °F
Lubrizol Advanced Materials PEARLCOAT® 125K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 125K is a polyester based TPU, supplied in form of translucent, colorless pellets, featuring medium softening point, and consistent quality pellets, low gel content as well low-tempera..
Zone 3 170 - 180 °C
338 - 356 °F
Lubrizol Advanced Materials PEARLCOAT® 168K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 168K is a polyether-based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low-temperature flexibility and very good hydrolysis resistance..
Zone 3 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin
Flame Retardant; Good UV Resistance; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsExtrusion equipment: st..
Zone 3 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Polidan® EC/110 Polyethylene, Crosslinked (XLPE)
Polidan® XLPE-PEX -Cross-linkable Polyethylene. Low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be use..
Zone 3 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Polidan® EC/51 Polyethylene, Crosslinked (XLPE)
Flexible low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards com..
Zone 3 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Polidan® EC/MD Polyethylene, Crosslinked (XLPE)
Medium density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards complying..
Zone 3 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Polidiemme® G/420 Thermoset Elastomer (TSE)
Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Si..
Zone 3 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties withou..