Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 199 - 221 °C | 390 - 430 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N80 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N80 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties and excellent hydrolys.. |
|||
Zone 3 | 199 - 221 °C | 390 - 430 °F | |
Ravago Manufacturing Americas Hylac® EX28 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Zone 3 | 199 - 216 °C | 390 - 420 °F | |
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra.. |
|||
Zone 3 | 199 °C | 390 °F | Extrusion |
Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane Features: High stiffness TPU alloyUses: Flat Die/Cast Sheet Extrusion, Profile Extrusion and Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided b.. |
|||
Zone 3 | 199 - 221 °C | 390 - 430 °F | |
Entec Hylac® EX18 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |