Processing Properties Metric English Comments
Zone 2 345 - 365 °C
653 - 689 °F
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres
Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca..
Zone 2 345 - 365 °C
653 - 689 °F
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified
Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca..