Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 270 - 285 °C | 518 - 545 °F | |
Nilit Nilamid A3 H ZB High Impact PA66 Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas .. |
|||
Zone 2 | 270 - 285 °C | 518 - 545 °F | |
Nilit Nilamid A3 H ZC High Impact PA66 Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Zone 2 | 270 - 285 °C | 518 - 545 °F | |
Nilit Nilamid A3 H ZE High Impact PA66 Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength.. |
|||
Zone 2 | 275 - 285 °C | 527 - 545 °F | |
Eurostar Starflam RF023P PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0023P is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding (also known as Starflam PA66C U2 Z23)Information provided by Eurostar. |
|||
Zone 2 | 260 - 285 °C | 500 - 545 °F | Center Zone |
BASF Ultramid® TG3S 15% Glass Filled PA6 (Dry) Description: Ultramid TG3S is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a ba.. |
|||
Zone 2 | 260 - 285 °C | 500 - 545 °F | Center Zone |
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Dry) Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the.. |
|||
Zone 2 | 260 - 285 °C | 500 - 545 °F | Center Zone |
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Conditioned) Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the.. |