Zone 2 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Zone 2 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Zone 2 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..
Zone 2 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a pol..
Zone 2 120 - 150 °C
248 - 302 °F
Solvay Specialty Polymers Polidiemme® G/400 Thermoset Elastomer (TSE)
Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Sioplas® method).Standards complying: Cenelec H..
Zone 2 120 - 150 °C
248 - 302 °F
Solvay Specialty Polymers Polidiemme® G/440 Thermoset Elastomer (TSE)
Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Sioplas® method)Standards complying: Cenelec HD..
Zone 2 120 - 150 °C
248 - 302 °F
Solvay Specialty Polymers Polidiemme® G/450 Thermoset Elastomer (TSE)
Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S..
Zone 2 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/370 Polyolefin, Unspecified  (discontinued **)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Copyright © lookpolymers.com All Rights Reserved