Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 255 °C | 491 °F | Compression |
BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |
|||
Zone 2 | 255 °C | 491 °F | Compression |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled PBT Description: Is a PBT, easy-flowing injection-molding grades with 15% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers, cove.. |
|||
Zone 2 | 255 °C | 491 °F | Compression |
BASF Ultradur® B 4330 G6 HR 30% Glass Filled PBT Description: Is a PBT-I, injection-molding grade with 30% glass fibers, for rigid, tough and dimensionally stable technical parts with increased requirements on hydrolysis resistance and toughness, .. |
|||
Zone 2 | 255 °C | 491 °F | Compression |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT Description: injection-molding grade with 30% glass-fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance. For example automotive connectors.. |