Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 235 °C | 455 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Zone 2 | 235 °C | 455 °F | Extrusion Coating |
DuPont™ Nucrel® 3990L Ethylene Acrylic Acid Nucrel® 3990L is a copolymer of ethylene and acrylic acid. It is available for use in conventional extrusion coating, coextrusion coating and extrusion laminating equipment. 9.5 % By Weight Acrylic.. |
|||
Zone 2 | 235 - 245 °C | 455 - 473 °F | |
Eurostar Star L PA D51 PA6, Injection Molded Star L PA6 D51 is a 15% PTFE Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 235 - 245 °C | 455 - 473 °F | |
Eurostar Starflam P10002Z PA6, Flame Retardant, Extrusion Starflam P10002Z is an Unfilled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Extrusion ResinInformation provided by Eurostar. |