Processing Properties Metric English Comments
Zone 1 120 - 130 °C
248 - 266 °F
Lubrizol Advanced Materials Pearlbond® 12C75 Thermoplastic Polyurethane
Pearlbond® 12C75 is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low softe..
Zone 1 120 - 130 °C
248 - 266 °F
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane
Pearlbondâ„¢ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ..
Zone 1 120 - 130 °C
248 - 266 °F
Lubrizol Advanced Materials Pearlthane® 12C75 Thermoplastic Polyurethane Elastomer
Pearlthane® 12C75 is a standard polyester based TPU supplied in form of translucent, colorless pellets, specially designed for compounds in which TPU is used as an additive. Features include low ..
Zone 1 120 - 130 °C
248 - 266 °F
Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 125H is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low soft..