Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020GX9 23% Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: 23% glass fiber reinforced gradeInformation provided by UBE. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020IX1 Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, impact modifiedInformation provided by UBE. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI5L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet SAE J844, DIN73378 HIPHLInformation provided by UBE. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JLX1 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 Description: UBESTA has a strong resistance to chemicalsInformation provided by UBE. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Nitric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hexane for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030UFX1 Rigid Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3035JU5 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, heat resistanceInformation provided by UBE. |
|||
Zone 1 | 230 - 240 °C | 446 - 464 °F | |
Eurostar Staramide PF005 PA6, 25% Glass Fiber Filled, Injection Molded Staramide PF005 is an 25% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 230 - 240 °C | 446 - 464 °F | |
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 230 - 240 °C | 446 - 464 °F | |
Eurostar Starflam B28UL PA6, Flame Retardant, Injection Molded Starflam B28UL is Unfilled Halogen Free and Red Phosphorous Free, Flame Retardant, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methanol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |