Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 199 °C | 390 °F | Zone 2 |
Premix Thermoplastics PRE-ELEC® ESD 7100 PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP 1227D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1274G Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1442A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1518C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1538A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1580B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1644L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1650L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1652B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1709C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1823 AS Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1881B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2100 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2100-S-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2103 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2111S-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2250 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2264R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP 1187 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1351J Thermoplastic Elastomer Uses: Consumer Applications; Gaskets; Plumbing Parts; Pump Parts Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a p.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1353A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1855V-NT Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2760BR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2870M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 °C | 390 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection .. |
|||
Die Temperature | 199 °C | 390 °F | Extrusion |
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2676B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2730 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 °C | 390 °F | Extrusion |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |