Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 190 - 210 °C | 374 - 410 °F | Average value: 197 °C Grade Count:7 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Die Temperature | 195 - 210 °C | 383 - 410 °F | Extrusion |
Stellarchem GP-945 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Die Temperature | 195 - 210 °C | 383 - 410 °F | Extrusion |
Stellarchem MP-850 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® OBC 4545A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1025-65 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1446G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1642E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1934G Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Connectors; Wire Jacketing; Wire and Cable Applications Agency Ratings: UL 1581Forms: Pellets Proces.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2318G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2478H Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2519G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2563A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-83-F912-ER Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-88-N873K BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-86-K986T-98 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |