Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 250 °C | 482 °F | Cast film |
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties.. |
|||
Die Temperature | 250 °C | 482 °F | Cast film |
DuPont Elvaloy® 3107 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3107 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3107 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |
|||
Die Temperature | 250 °C | 482 °F | For high temperature coextrusions. |
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Die Temperature | 250 °C | 482 °F | For high temperature coextrusions. |
DuPont Bynel® 50E662 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E662 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion an.. |